Polymer Property : Tear Strength = 91.3 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 12.0 - 16.0 kN/m
68.5 - 91.3 pli
NF EN ISO 1421
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Tear Strength 12.0 - 16.0 kN/m
68.5 - 91.3 pli
NF EN ISO 1421
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.