Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 2.00 - 113 kN/m | 11.4 - 645 pli | Average value: 24.8 kN/m Grade Count:768 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |