Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 175 kN/m | 999 pli | DIN 53515 |
Lubrizol ESTANE® X1013 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 175 kN/m | 999 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 175 kN/m | 999 pli | |
AorTech Biomaterials ECSil™ 70D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |
|||
Tear Strength | 175 kN/m | 999 pli | |
AorTech Biomaterials ECSil™ 70D Biomedical Carbonate Silicone Pellets Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an.. |