Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 16.0 kN/m | 91.3 pli | Die B |
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3440 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ASTM D624 |
ELASTO UK Dryflex® 500300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Injection Molding, Pebble Gray Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 16.0 - 37.0 kN/m | 91.3 - 211 pli | ASTM D 624 |
API Megol AM DP2339 SEBS Adhesion Modified Overmolding for PA Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 34-B |
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3140 can be processed by injection molding or extrusion for appl.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | |
Trelleborg Commercial Neoprene® C803 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | angle |
Momentive Performance Materials XE23-703U Heat Cured Rubber - Electro Conductive Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 16.0 kN/m | 91.3 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5696 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |