Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 14.9 kN/m | 85.0 pli | ASTM D624 |
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | ASTM D624 |
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-330A Solid Polyurethane Elastomer TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3 Basic PTFE-Coated Glass Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barr.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, g.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: .. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® XF-200 Fully Sintered PTFE Coated, Flexible, Non-porous Fluoropolymer Laminated Composite Description: Chemlam® is the trademark for the Chemfab® family of flexible, non-porous fluoropolymer laminated composites that combine the features of multi-layer fluoropolymer cast films with.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | |
Dow Corning SILASTIC® M-2 RTV SILICONE RUBBER BASE & CURING AGENT High durometer mold making silicone rubber suited for the reproduction of architectural, furniture components and prototypes. Silastic M is recommended for use with rigid and foam polyurethane and c.. |
|||
Tear Strength | 14.9 kN/m | 85.0 pli | |
BCC Products BC 9040 T Silicone RTV Rubber BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high.. |