Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 145 kN/m | 827 pli | Die C; ASTM D624 |
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Tear Strength | 145 kN/m | 827 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR5225 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 145 kN/m | 827 pli | ASTM D1004 |
SK Chemicals SKYPEL P155D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |