Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 127 kN/m | 725 pli | Die C; ASTM D624 |
Northstar Polymers MSS-A85C Ester Base Polyurethane This high performance polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhibit hig.. |
|||
Tear Strength | 127 kN/m | 725 pli | |
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping.. |
|||
Tear Strength | 127 kN/m | 725 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 127 kN/m | 725 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 127 kN/m | 725 pli | without incision; ISO 34B |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 127 kN/m | 725 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR5260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |