Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 109 kN/m | 620 pli | Die C |
Elastomer Engineering E50D Polyurethane A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elasto.. |
|||
Tear Strength | 109 kN/m | 620 pli | ASTM D624 |
Dow SPECTRIM™ 50-S Reaction Moldable Polymer SPECTRIM™ 50-S reaction moldable polymer is a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology developed by the Dow Chemical Company.Information p.. |