Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 185A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 190A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® X585A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 585A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
Lubrizol Estane® S185A Thermoplastic Polyurethane Type: Estane® S185A is a Shore 87A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Prov.. |
|||
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
Toyobo PELPRENE™ P95C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Tear Strength | 108 kN/m | 616 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP95AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses:Injection molding partsAvailable in EuropeInformation provided by.. |
|||
Tear Strength | 108 kN/m | 616 pli | Die C; ASTM D624 |
Lubrizol Estane® R190A Thermoplastic Polyurethane Type: Estane® R190A is a Shore 93A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provi.. |
|||
Tear Strength | 108 kN/m | 616 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR9020 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |