Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.5 kN/m | 59.9 pli | ASTM D624B |
P & P Technology CB 50 Carbon Loaded Silicone Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,.. |
|||
Tear Strength | 10.5 kN/m | 59.9 pli | |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Tear Strength | 10.5 kN/m | 59.9 pli | |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Tear Strength | 10.5 kN/m | 59.9 pli | |
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Tear Strength | 10.5 kN/m | 59.9 pli | ASTM D624 |
Teknor Apex Uniprene® UN-2533A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 10.5 kN/m | 59.9 pli | ASTM D624 |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |