Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 98.2 kN/m | 560 pli | Die C; ASTM D624 |
Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | ASTM D624 |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Kostat Method |
Kostat KAH1 Heat Seal Activated Cover tapes KOSTATs KAH1 series of Heat Seal Activated Cover Tape is manufactured using Antistatic Polyethylene Terephthalate film and other proprietary adhesive materials. The component for its anti-static pr.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 180A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 185A L series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Initial Tear Strength; ASTM D-1004 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 98.1 kN/m | 560 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 10 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 98.2 kN/m | 560 pli | ASTM D624 |
Buckeye Polymers BP Flex D0853 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 10 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |