Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 62.9 kN/m | 359 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9002 GREY/BROWN Ash is 15%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 62.9 kN/m | 359 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 62.9 kN/m | 359 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 62.9 kN/m | 359 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 20 Minutes Milling MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, No Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 62.9 kN/m | 359 pli | Die C; ASTM D624 |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 63.0 kN/m | 359 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 90A, Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |