Mechanical Properties Metric English Comments
Tear Strength 55.9 kN/m
319 pli
Die C, 2 in/min; ASTM D1004
PolyOne Geon™ Vinyl Flexible 90057 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne