Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 54.9 kN/m | 313 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 54.9 kN/m | 313 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7090-1000 TPE Product Description: StarMediflex P 7090-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 54.9 kN/m | 313 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |