Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 54.0 kN/m | 308 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9305 BLK This product was developed for one shot airbag covers with improved stiffness and low temperature resistance. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 54.0 kN/m | 308 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | Trouser Tear Resistance, MD; ISO 6383-1 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Tear Strength | 53.9 kN/m | 308 pli | 50mm/min, @ Break; ASTM D624 |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Tear Strength | 54.0 kN/m | 308 pli | Die B, no post cure; ASTM D624 |
Multibase C6-570 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 54.0 kN/m | 308 pli | ASTM D624 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | ASTM D2240 |
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | DIN 53515 |
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 54.0 kN/m | 308 pli | GB/T 529 |
Chengdu Polyster 8500 General Grade TPV Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 54.0 kN/m | 308 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tear Strength | 54.0 kN/m | 308 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ GF 6257 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 54.0 kN/m | 308 pli | Trouser Tear Resistance, MD; ISO 6383-1 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |