Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 51.0 kN/m | 291 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8000 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 51.0 kN/m | 291 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8002 BLK Multi-Flex® TPE 8002 is based on Shell's Kraton G polymer technology and is widely used in the automotive industry for applications requiring elastomeric performance with excellent ozone resistance.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die B, post cured- 4 hours at 200°C; ASTM D624 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 51.0 kN/m | 291 pli | ISO 34 |
Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | B-type, Vulcanized |
KKPC KOSYN 1502 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3480N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | ASTM D624 |
UBE UBEPOL BR150L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TP-759 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | GB/T 529 |
Chengdu Polyster 7502 High Performance Grade TPV Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 51.0 kN/m | 291 pli | ASTM D624 |
BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ BF-30 Woven Fabric 440 Information provided by 3M |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.5 PHR Varox DBPH-50 Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 51.0 kN/m | 291 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3180 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3180 can be processed by blow molding injection molding or ex.. |