Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 50.0 kN/m | 285 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90031 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 50.0 kN/m | 285 pli | |
Huntsman IROGRAN® A 85 P 4666 Ether-Based TPU-For Cable Industry HFFR, radiation cross-linkableInformation provided by Huntsman |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | DIN 53507 |
Karina 701D48/1-A-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | DIN 53507 |
Karina 722-48/1-A-IS Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automobile profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2661 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN 53515 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ISO 34 |
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE) Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 502850S SEBS Based Material, Unfilled Qualities, 85A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D624 |
ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Tear Strength | 49.9 - 58.6 kN/m | 285 - 335 pli | ASTM D624 |
3M 32662 Black Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 60 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 50.0 kN/m | 285 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 70 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 50.0 - 70.0 kN/m | 285 - 399 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | ASTM D 624 |
API Megol AM DP2217/90PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 49.9 - 58.6 kN/m | 285 - 335 pli | ASTM D624 |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | ISO 34 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | >= 50.0 kN/m | >= 285 pli | ISO 34 |
Austin Novel Materials Texalan® 570A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | 50.0 - 70.0 kN/m | 285 - 399 pli | TM-019K |
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in .. |
|||
Tear Strength | 50.0 kN/m | 285 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-550 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 49.9 kN/m | 285 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 49.9 - 58.6 kN/m | 285 - 335 pli | ASTM D624 |
3M 32664 Light Gray Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |