Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.38 kN/m | 25.0 pli | ASTM D624 |
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | ASTM D624 |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Split; ASTM D624 |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Die C; ASTM D624 |
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2265-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® HM350 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® HM426 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M64 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M705 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M706 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M716 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M751 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M758 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M765 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M797 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M803 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M815 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M823 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M827 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M851 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M97 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M50 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M56 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low water absorptio.. |
|||
Tear Strength | 4.38 kN/m | 25.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M54 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |