Polymer Property : Tear Strength = 245 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 42.9 kN/m
245 pli
Die C, 510 mm/min; ASTM D624
PolyOne Synprene® RT-5180 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tear Strength 43.0 - 59.0 kN/m
245 - 337 pli
NF EN ISO 1421
Isoflon Tisoflon® 24S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Addisilâ„¢ 1050 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Addisilâ„¢ 1140 M Industrial Molding Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Addisilâ„¢ 2050 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LIM 6050 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Addisilâ„¢ 450 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 43.0 kN/m
245 pli
Die B
Momentive Performance Materials Addisilâ„¢ 452 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 42.9 kN/m
245 pli
Die C
Taiwan PU Corporation UR70 Polyester Urethane Rubber
UR70 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of ..
Tear Strength 42.9 kN/m
245 pli
ASTM D624
Teknor Apex Monprene® MP-1627I Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tear Strength 42.9 kN/m
245 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR Di-Cup 40C Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 43.0 kN/m
245 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 42.9 kN/m
245 pli
Die C
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR Di-Cup 40C Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..