Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 37.3 kN/m | 213 pli | as molded; Die B |
Multibase SILASTIC® C7-4550 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 37.3 kN/m | 213 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 37.3 kN/m | 213 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 37.4 kN/m | 213 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 5401 BLK Ash is 4.71%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 37.3 kN/m | 213 pli | ASTM D412 |
Stellarchem SV-B80E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Tear Strength | 37.3 kN/m | 213 pli | DIN 53363 |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Tear Strength | 37.3 kN/m | 213 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 37.3 kN/m | 213 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 37.3 kN/m | 213 pli | kg/cm²; JIS-K-6301 |
Denka LCS Z1070 Thermoplastic Elastomer, Extrusion grade (general) "DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r.. |