Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 35.0 kN/m | 200 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO A-7507 TPO compound suitable for carpet backing seals.Data provided by Multibase. |
|||
Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
Network Polymers Softflex® 6500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible C70U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 35.0 kN/m | 200 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene LDPE 2501TN00 Hygienic Film It is used in diaper film, lamination film and in applications where low blocking behavior without the help of additives is required.Information provided by Iran Petroch.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Addisilâ„¢ 440 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
Karina E 65/225 Compound PVC Crystal Crystal PVC compound, recommended for injection of shoe/sandal industry.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 35.1 kN/m | 200 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 1115 Abrasion Resistant Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 35.0 kN/m | 200 pli | GB/T 529 |
Chengdu Polyster 5502 High Performance Grade TPV Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 35.1 kN/m | 200 pli | 73°F, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | |
Arlon 10842N125 Cured/Post-cured, Unsupported Silicone Rubber Low ModulusProduct Color: Natural (Transparent)Interleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Inform.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | Compound Property |
Arlon 10842S020 0.020" (0.508 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | |
Arlon 10842S090 Fully Cured, Unsupported Silicone Rubber Product Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by AR.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | Silicone Property |
Arlon 30400N085 0.085" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | Compound Property |
Arlon 30400N125 0.125" (3.17 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Kodacel Carrier Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the production ma.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | Silicone Property |
Arlon 30400R040 0.04" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | |
Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020) Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave.. |
|||
Tear Strength | 35.1 kN/m | 200 pli | |
BCC Products DP-11-83 Urethane Adhesive-Slo DP-11-83 is a low viscosity, quick setting, easy to use adhesive and/or casting material. This product was designed to bond together the MB1200 foam board to create desired dimensions in length, wid.. |
|||
Tear Strength | 35.1 kN/m | 200 pli | Die C; ASTM D624 |
Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Tear Strength | 35.0 kN/m | 200 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 35.1 kN/m | 200 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tear Strength | >= 35.1 kN/m | >= 200 pli | Silicone Property |
Arlon 30850N125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |