Mechanical Properties Metric English Comments
Tear Strength 0.430 kN/m
2.45 pli
ASTM D 624
Eurofoam Porocell POR 303/B GR CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..
Tear Strength 0.430 kN/m
2.45 pli
ASTM D 624
Eurofoam Porocell POR 303/B RS CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..
Tear Strength 0.430 kN/m
2.45 pli
ASTM D 624
Eurofoam Porocell POR 303/B CR-Neoprene/NBR Foam
Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam..