Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 0.380 kN/m | 2.17 pli | ASTM D 624 |
Eurofoam Porocell POR 302/T-E NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |