Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 34.1 kN/m | 195 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7101 BLK Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 34.1 kN/m | 195 pli | ASTM D624 |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tear Strength | 34.1 kN/m | 195 pli | ASTM D624 |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tear Strength | 34.1 kN/m | 195 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 34.1 kN/m | 195 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 60 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 34.2 kN/m | 195 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerApplications:General PurposeCove BaseInteriorMarket:AutomotiveConsumer GoodsBuilding and ConstructionProcessing Method:Extrusion and Molding.. |