Mechanical Properties Metric English Comments
Tear Strength 27.5 kN/m
157 pli
Die B, post cured- 4 hours at 200°C; ASTM D624
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 27.5 kN/m
157 pli
ASTM D624
Network Polymers Softflex® 5300
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tear Strength 27.5 kN/m
157 pli
ASTM D624
Network Polymers Softflex® 5500
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tear Strength 27.5 kN/m
157 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 27.5 kN/m
157 pli
Die B, no post cure; ASTM D624
Multibase C6-530 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 27.5 kN/m
157 pli
500 mm/min; ASTM D 624
Zylog Neoplast® 173 C Thermoplastic Vulcanizate
Neoplast 173 C is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV S..
Tear Strength 27.5 kN/m
157 pli
500 mm/min; ASTM D 624
Zylog Neoplast® 173 FT EB Thermoplastic Vulcanizate
Neoplast 173 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro..
Tear Strength 27.5 kN/m
157 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 27.5 kN/m
157 pli
Dow Corning 25150-G SILICONE RUBBER
Peroxide cured, general purpose silicone rubber compoundInformation provided by Dow Corning