Polymer Property : Tear Strength = 153 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 26.8 kN/m
153 pli
as molded; Die B
Multibase SILASTIC® C7-4535 VAROX Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 26.8 kN/m
153 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-1 TPE
Product Description: StarTUFF TF 45-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..