Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.3 kN/m | 150 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | die C; ASTM D624 |
PB1100-60 Polyurethane-based Biomedical Elastomer |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, Silicone Property; ASTM D624 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7375-9000 TPE Product Description: StarFlex P 7375-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG15-05(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 8 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material Description: General Notes on Saint Gobain Chemfab® TCN® Open Mesh Belting Products:TCN belting products are PTFE coated Nomex®, a high-temperature polyamide fiber that maintains its struct.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 1 Uncured Silicone Property; ASTM D624 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Layer 2, Silicone Property; ASTM D624 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624C-73 |
3M SJ-3A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; Arlon SQA-TMS-029 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624-73 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624-73 |
3M 8462 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3850M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B; Silicone Property; ASTM D624 |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3840E Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionPolyOne First ChoiceDisclaimer: A ther.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® q-GUARD® 112 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fiberglas.. |