Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 245 - 316 kN/m | 1400 - 1800 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tear Strength | 245 - 316 kN/m | 1400 - 1800 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Tear Strength | 245 - 316 kN/m | 1400 - 1800 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Tear Strength | 245 - 316 kN/m | 1400 - 1800 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Tear Strength | 245 kN/m | 1400 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 168D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 245 kN/m | 1400 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S168D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 245 kN/m | 1400 pli | Die C; ASTM D624 |
Lubrizol Estane® S168D Thermoplastic Polyurethane Type: Estane® S168D is a Shore 68D, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Tear Strength | 245 kN/m | 1400 pli | ASTM D624 |
Toyobo A1064D Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tear Strength | 245 - 316 kN/m | 1400 - 1800 pli | initiation; ASTM D1004 |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |