Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 6821 NAT This product is based on Kraton G and PP. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® TPE RP 6568 C340 BLK This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. Ash is 2.2%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided .. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D412 |
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D412 |
Multibase TPSiV™ 3040-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Tear Strength | 24.5 - 26.5 kN/m | 140 - 151 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9885/9785 Rubber-like Prototyping Polymer Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7370-1000 TPE Product Description: StarFlex P 7370-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C; ASTM D624 |
Teknor Apex APEX® 3055-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Initial Tear Strength; ASTM D1004-94 |
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tub.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 24.5 kN/m | 140 pli | |
Dow Corning SILASTIC® 3497 MOULD MAKING BASE & 96 CURING AGENT High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | |
Dow Corning SILASTIC® 7-6830 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 24.5 kN/m | 140 pli | |
Dow Corning SILASTIC® S RTV SILICONE RUBBER BASE & GREEN CURING AGENT High strength silicone rubber suited for prototyping, production tooling, artistic and renovation applications. Silastic S is recommended for use with polyesters, cement and rigid polyurethanes; als.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | at 25°C |
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Diamond Polymers Softflex® 4550 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Warp, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 702 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat.. |