Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 23.1 kN/m | 132 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7360-1000 TPE Product Description: StarFlex P 7360-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 23.1 kN/m | 132 pli | ASTM D624 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |