Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 23.0 kN/m | 131 pli | D624 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5G Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 6G EXTRA SMOOTH QUALITY Polytetrafluoroethylene & Graphite Coated Glass Fabric PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tear Strength | 23.0 - 24.0 kN/m | 131 - 137 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 10S Silicone Coated Glass Fabric Silicone coated Glass fabric TISOFLON®Information provided by Isoflon. |
|||
Tear Strength | 23.0 - 26.0 kN/m | 131 - 148 pli | NF EN ISO 1421 |
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Press-cured 5 minutes at 190°C; ISO 34 |
DuPont Vamac® DP HVA-2 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
Trelleborg E669 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
Trelleborg E666 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Black, Halogen Free Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Injection Molding, Natural, Halogen Free Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | Die B; Silicone Property; ASTM D624 |
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | |
ACC MM928 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 221-64W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed .. |
|||
Tear Strength | 23.0 kN/m | 131 pli | 73°C, Die C, Across Flow; ASTM D624 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |