Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 22.6 kN/m
129 pli
post cured- 4 hours at 177°C; Die B
Multibase SILASTIC® Q7-4780 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength <= 22.6 kN/m
<= 129 pli
Die C; Formulation Example; Press Cure 7'/177ºC
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
Tear Strength 22.6 kN/m
129 pli
ASTM D412
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Tear Strength <= 22.6 kN/m
<= 129 pli
Die C; Formulation Example; Press Cure 7'/177ºC
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
Tear Strength 22.6 kN/m
129 pli
Dow Corning SILASTIC® LC-20-2004 PART A&B KIT
20 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber. Fast curing speed, long pot life (72 hours), high transpa..
Tear Strength 22.6 kN/m
129 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
Tear Strength 22.6 kN/m
129 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M