Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 201 - 250 kN/m | 1150 - 1430 pli | |
Taiwan PU Corporation PTMG CPU-325L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Tear Strength | 201 kN/m | 1150 pli | Die C; ASTM D624 |
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat.. |