Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.0 kN/m | 114 pli | |
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
Tear Strength | >= 20.0 kN/m | >= 114 pli | DIN 53507 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | >= 20.0 kN/m | >= 114 pli | DIN 53507 |
Karina E CAK 85-48/1-F Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7586/40 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FSL 7651 Fluorinated Liquid Silicone Rubber This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 4070 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tear Strength | 20.0 kN/m | 114 pli | angle |
Momentive Performance Materials XE23-B2484 Heat Cured Rubber - Electro Conductive Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7060-1000 TPE Product Description: StarMediflex P 7060-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg B574 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg E849 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg R572 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S650 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S765 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S850 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg Neoprene® C626 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Dryflex® 402501S SBS Based Material, 50A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ASTM D624 |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ISO 34-B |
AlphaGary Evoprene™ Super G 948 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | |
Trelleborg S763 Silicone Rubber PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering... |
|||
Tear Strength | 20.0 - 30.0 kN/m | 114 - 171 pli | Die B; ASTM 624 |
Wacker Silicones Geniomer® 80 Silicone TPE SLM TPSE 80 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |
|||
Tear Strength | 20.0 kN/m | 114 pli | ISO 4674-1 Method B |
Rogers Corporation Bisco® A2 R 1.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |
|||
Tear Strength | 20.0 - 373 kN/m | 114 - 2130 pli | Average value: 79.8 kN/m Grade Count:15 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |