Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 6.30 - 104 kN/m | 35.9 - 593 pli | Average value: 34.6 kN/m Grade Count:26 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Tear Strength | 22.0 - 104 kN/m | 126 - 593 pli | Average value: 54.1 kN/m Grade Count:8 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |