Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 98.1 kN/m | 560 pli | ASTM D624 |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Kostat Method |
Kostat KAH1 Heat Seal Activated Cover tapes KOSTATs KAH1 series of Heat Seal Activated Cover Tape is manufactured using Antistatic Polyethylene Terephthalate film and other proprietary adhesive materials. The component for its anti-static pr.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 180A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 185A L series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® L185A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Initial Tear Strength; ASTM D-1004 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 98.1 kN/m | 560 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 10 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 98.1 kN/m | 560 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 10 PHR Tricresyl Phosphate MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |