Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | <= 9.64 kN/m | <= 55.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL® 6452 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-220A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2042-10 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Silicone Property; ASTM D624 |
Arlon 10292R062 Cured Silicone Rubber (Unsupported) with Polyethylene Liner Design/Construction:Material: Cured Silicone RubberLiner: PolyethyleneRecommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicone.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Silicone Property; Die B; ASTM D624 |
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Side 1 Cured Silicone Property; ASTM D624 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R34570R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1080 Style FiberglassThis data represents typical values for the production material. The data should no.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R34572R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1080 Style FiberglassAppearance: Red silicone rubber on fiberglass clothThis data represents typical value.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Silicone, Die B; ASTM D624 |
Arlon 54B12R006 Silicone Rubber/Fiberglass Laminate Cured silicone rubber with a fiberglass substrate. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon R3758R0055 0.065" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Tear Strength | 9.64 kN/m | 55.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |