Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 85.0 kN/m | 485 pli | Injection molded parts; DIN 53515 |
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN 53515 |
Lubrizol ESTANE® X4928 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 85.0 kN/m | 485 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-A890 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN 53515 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | with incision; ISO 34B |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | with incision; ISO 34B |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN 53515 |
Lubrizol ESTANE® 5701F1 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN 53515 |
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN 53515 |
Lubrizol ESTANE® 58447 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 85.0 kN/m | 485 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 9035-101 TPE, Modified Injection Molding Grade for Semi Rigid Molding The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 9035-101 is specifically designe.. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN ISO 34-1/Bb |
BASF Elastollan 690 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 85.0 kN/m | 485 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tear Strength | 85.0 kN/m | 485 pli | ASTM D624 |
BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tear Strength | 85.0 kN/m | 485 pli | ASTM D624 |
BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tear Strength | >= 85.0 kN/m | >= 485 pli | ISO 34 |
Austin Novel Materials Texalan® 490A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | >= 85.0 kN/m | >= 485 pli | ISO 34 |
Austin Novel Materials Texalan® 582A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tear Strength | >= 85.0 kN/m | >= 485 pli | ISO 34 |
Austin Novel Materials Texalan® 790A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | >= 85.0 kN/m | >= 485 pli | ISO 34 |
Austin Novel Materials Texalan® 385A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tear Strength | 85.0 kN/m | 485 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |