Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 78.8 kN/m | 450 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 78.8 kN/m | 450 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL 0131-61 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tear Strength | 78.8 kN/m | 450 pli | Die C; ASTM D624 |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Tear Strength | 78.8 kN/m | 450 pli | ASTM D624 |
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro.. |
|||
Tear Strength | 78.8 kN/m | 450 pli | ASTM D624 |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |