Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 77.0 kN/m | 439 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90253 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 77.0 kN/m | 439 pli | Die C, 2 in/min; D1004 |
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **) Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201.. |
|||
Tear Strength | 77.0 kN/m | 439 pli | 100 micron film; ASTM D1004 |
Kaneka PHBH Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Tear Strength | 77.0 kN/m | 439 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 3104-10 AGATE 5ES The material is based on Kraton G rubber. It has been engineered for single shot. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 77.0 kN/m | 439 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 3104-8 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 77.0 kN/m | 439 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 77.0 kN/m | 439 pli | ASTM D624 |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 77.0 kN/m | 439 pli | ASTM D624 |
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |