Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 75.3 kN/m | 430 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90453 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |