Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.50 kN/m | 42.8 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCA871 PPE-TPE (Asia Pacific) Halogen-free flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as insulation and cable jacket. Flame retardant performance and mechanical properties capable.. |