Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 68.3 kN/m | 390 pli | Die C, 51 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90212 Polyvinyl Chloride, Flexible (PVC, Flexible) Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne |
|||
Tear Strength | 68.3 kN/m | 390 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 68.3 kN/m | 390 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 3 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |