Mechanical Properties Metric English Comments
Tear Strength 61.4 kN/m
350 pli
Split; ASTM D624
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Tear Strength 61.4 kN/m
350 pli
Die 'C'; ASTM D624
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® thermoplastic siliconepolyether-urethane (TSPU) is a novel copolymer that is strong, yet flexible with proven biocompatibility and biostability. Leveraging the benefits of both silicone ela..
Tear Strength 61.4 kN/m
350 pli
Die C; ASTM D624
Northstar Polymers MGG-A70DQ High Performance Polyurethane Cast Elastomer System 70A
This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and..
Tear Strength 61.4 kN/m
350 pli
25 mil film; ASTM D624
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
Tear Strength 61.4 kN/m
350 pli
ASTM D624
Huntsman IROGRAN® PS455-203 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Tear Strength 61.4 kN/m
350 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-370A Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 61.4 kN/m
350 pli
ASTM D624
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black
Information provided by ITW Devcon
Tear Strength 61.4 kN/m
350 pli
ASTM D624
Multibase Multi-Flex® G 7827 Black TPE Styrene Ethylene Butylene Styrene Block Copolymer
Forms: PelletsProcessing Methods:Injection Molding Uses: Automotive ApplicationsInformation provided by Multibase
Tear Strength 61.4 kN/m
350 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-390A Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 61.4 kN/m
350 pli
Warp/Longitudinal direction; ASTM D1000
Saint-Gobain COHRlastic® 1025 General-Purpose Electrical-Grade Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..
Tear Strength 61.4 kN/m
350 pli
Warp/Longitudinal direction; ASTM D1000
Saint-Gobain COHRlastic® 3016 Low Temperature Flexibility Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..
Tear Strength 61.4 kN/m
350 pli
Fill/Transverse direction
Saint-Gobain COHRlastic® 3032 Low Temperature Flexibility Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 14 Primary PTFE-Coated Glass
Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: ..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Fill)
Saint-Gobain Chemfab® TCK® 1589 High-Strength Plain Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® TCK® 1589 High-Strength Plain Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Fill)
Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 61.4 kN/m
350 pli
Initial Tear Strength; ASTM D1004-93
Saint-Gobain Tygothane® C-544-AI.B. Precision Polyurethane Pressure Tubing Formulation
Description: Tygothane® C-544-A I.B.: More flexible than many other reinforced urethane tubings, Tygothane® Pressure Tubing can be used in some of the most physically demanding applications,..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 13 Premium PTFE-Coated Glass
Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 13 Tear Resistant PTFE-Coated Glass
Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting
Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® TCKGN Heavyweight Rough Surface Belting
Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi..
Tear Strength 61.4 kN/m
350 pli
Die C; ASTM D1004
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tear Strength 61.4 kN/m
350 pli
ASTM D412
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant
EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala..
Tear Strength 61.4 kN/m
350 pli
ASTM D2240
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti..
Tear Strength 61.4 kN/m
350 pli
ASTM D412
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..
Tear Strength 61.4 kN/m
350 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 14 High-Performance PTFE-Coated Glass
Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat s..