Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 58.7 kN/m | 335 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 9009 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 58.7 kN/m | 335 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene™ RT-5190 RoHS Black Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 58.7 kN/m | 335 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Di-Cup 40C Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 58.7 kN/m | 335 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR Di-Cup 40C Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |