Mechanical Properties Metric English Comments
Tear Strength 57.0 kN/m
325 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 57.0 kN/m
325 pli
Die B
Momentive Performance Materials TUFELâ„¢ II 94705 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 57.0 kN/m
325 pli
Die B
Momentive Performance Materials TUFELâ„¢ II 94706 Low Volatile Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 57.0 kN/m
325 pli
ISO 34-1
Green Dot Terratek® Flex GDH-B1 Compostable Bioplastic Elastomer
GDH-B1 is an elastomeric bioplastic with a diverse range of potential applications. It is a starch-based elastomer that is strong, durable and pliable with an exquisite soft touch. The bioplastic i..
Tear Strength 57.0 kN/m
325 pli
Die B
Momentive Performance Materials Addisilâ„¢ 1180 M Industrial Molding Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 57.0 kN/m
325 pli
ASTM D624
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black
Information provided by ITW Devcon
Tear Strength 57.0 kN/m
325 pli
Warp/Longitudinal direction
Saint-Gobain Chemlam® Silver 12 Wear Resistant Industrial Laminate
Description: The Chemlam® Silver series is the wear resistant line of Chemfab® industrial laminates. Chemlam® Silver composites feature uniform thickness, multi-layer cast PTFE films lamina..
Tear Strength 57.0 kN/m
325 pli
Warp/Longitudinal direction
Saint-Gobain Chemlam® XF-900 Fully Sintered PTFE Coated, Flexible, Non-porous Fluoropolymer Laminated Composite
Description: Chemlam® is the trademark for the Chemfab® family of flexible, non-porous fluoropolymer laminated composites that combine the features of multi-layer fluoropolymer cast films with..
Tear Strength 57.0 kN/m
325 pli
Initial Tear Strength
Saint-Gobain CHR® SG13-10(R) High Performance Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 57.0 kN/m
325 pli
Initial Tear Strength
Saint-Gobain CHR® SG15-10(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 57.0 kN/m
325 pli
Initial Tear Strength
Saint-Gobain CHR® SG16-10(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 57.0 kN/m
325 pli
Tensile Strength (Fill)
Saint-Gobain Chemfab® q-GUARD® 18 Insulation Jacketing
Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl..
Tear Strength 57.0 kN/m
325 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® TCK® 800 High-Strength Leno Weave Small Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 57.0 kN/m
325 pli
DIN 53515
Lubrizol ESTANE® T5134 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 57.0 kN/m
325 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 75A
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 57.0 kN/m
325 pli
GB/T 529
Chengdu Polyster 8502 High Performance Grade TPV
Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 57.0 kN/m
325 pli
Perpendicular to flow; ISO 34-B
AlphaGary Evoprene™ GF 6257 Automotive Thermoplastic Elastomer
Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Tear Strength 57.0 kN/m
325 pli
Perpendicular to flow; ISO 34-B