Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Multibase Multi-Flex® A 9402 AH Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 56.1 kN/m | 320 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 56.1 kN/m | 320 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7100-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 56.1 kN/m | 320 pli | Die C; ASTM D624 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
Tear Strength | 56.1 kN/m | 320 pli | |
Cytec EN-7 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Tear Strength | 56.1 kN/m | 320 pli | |
Cytec EN-8 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |