Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 49.6 kN/m | 283 pli | Die B, post cured- 4 hours at 166°C; ASTM D624 |
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 49.6 kN/m | 283 pli | ASTM D624 |