Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 48.1 kN/m | 274 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D-3120 Multi-Flex® TPO D-3120 is a compound for automotive applications replacing Himont's 7023. The burn rate is 0.87 in/min; ASTM FM VSS 30.Data provided by Multibase. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | ASTM D1004 |
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 48.1 kN/m | 274 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |