Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 46.0 kN/m | 262 pli | ISO 34-1 |
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94605 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tear Strength | 46.0 kN/m | 262 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tear Strength | 46.0 kN/m | 262 pli | ISO 6383 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Tear Strength | 46.0 kN/m | 262 pli | DIN 53515 |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 3.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | GB/T 529 |
Chengdu Polyster 6502 High Performance Grade TPV Excellent resiliency, good hand feel, paintable.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Across Flow, Die C; ASTM D624 |
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Across Flow, Method Bb, Angle (Nicked); ISO 34-1 |
ExxonMobil Santoprene® 291-75B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | ISO 34-B |
AlphaGary Evoprene™ 049 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | Die B |
Momentive Performance Materials TUFEL™ II 94606 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 46.0 kN/m | 262 pli | ISO 34-B |
AlphaGary Evoprene™ GC 640 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |